Hard Anodising Adhesion and Bond Strength
While anodising successfully is crucial to the part functioning correctly after coating, it is easy to fail to achieve good adhesion. What determines the potential for good adhesion? The answer relates to the characteristics of the metal to be anodised, the surface and the part geometry.
Why It Grows From The Metal
The process of hard anodising is not one of applying a paint or coating to aluminium surfaces. Instead the anodising process grows an oxide layer from within the metal itself. This layer is formed by converting the top portion of the metal into aluminium oxide. In fact the anodising process forms a bond between the oxide layer and the aluminium so strong that it is virtually impossible to remove the layer without dissolving the metal itself. This is explained in more detail on the Royal Society of Chemistry’s web site about how oxide layers are formed on metal surfaces.
Alloy Choice Matters More Than You’d Think
Wrought alloys such as 6061 or 6082 tend to anodize well because they have a fine even grain structure. This allows the oxide to grow in a uniform manner. High-copper alloys such as 2014 or 2024 and some high-silicon casting alloys are more difficult to anodize. This is because copper and silicon do not convert to oxide in the same manner as aluminium and so become trapped within the growing layer. Such a layer is more brittle and prone to cracking. The anodic oxide formed on such alloys can also be patchy and poor adhesion can occur, particularly with cast components.
Surface Preparation Makes Or Breaks It
Degreasing: This stage removes oils and other dirt and residues that have attached themselves to the part during transport and storage. Anodising processes cannot start until all surfaces have been degreased. Alkaline Etching: The surface of the part must be cleaned to remove the natural surface film (oxide skin). This produces a rough surface which the anodising process can then build upon. The etched surface has a dark sooty appearance and this is made up of the alloying elements in the aluminium that the etch solution has not dissolved. These must be desmutted from the surface of the part prior to anodising, using a desmutting dip solution (typically a nitric acid or mixed acid solution).
Current Density And Bath Temperature Control The Oxide Structure

A process operating at low temperature (approximately 0°C to 5°C) with carefully controlled current density produces a dense, fine-pored structure, very hard with good adhesion. An anodizing process operating at too high a temperature or current density produces a layer of faster growth rate with a looser, larger-pored structure, which whilst very hard is poor in adhesion to the base metal and will wear rapidly.
Warning Signs Of Poor Adhesion
A well-bonded layer is smooth and even with an even, matt grey colour. Poor adhesion will lead to flaking at edges and corners. There may also be signs of poor adhesion such as a powdery or even chalky surface which will rub off with a finger. In extreme cases blisters may form due to gas evolution within the layer. In some instances burning may occur (smooth patches of dark colour). These are problems that have arisen due to defects in the metal, surface preparation or anodizing process and cannot be fixed by subsequent anodizing.
How Adhesion Gets Checked
Adhesion testing: A simple test for the adhesion of anodised layers is to remove tape from the anodised surface. If the tape pulls off layers of anodising then clearly the adhesion has not been good. More rigorous testing can include bend testing of test strips (to look for cracking or loss of adhesion on bending) and examination of polished cross-sections of the anodised part under a microscope to determine the thickness of the anodic layer. Importantly it will also show if the layer is dense and continuous with no sign of porosity or remaining smut within the layer.
Design Features That Create Weak Spots
Sharp internal radii, welds, deep machined features and surface irregularities all present special challenges for good anodic adhesion. Such features concentrate local stresses during anodising, and so grow thinner, possibly more brittle, anodic layers than would be produced on flat surface areas. Designers must be aware of these potential problems and take steps to avoid them by specifying, for example, a small radius on internal corners.
Handling Parts After Anodising
Hard anodic coatings are extremely hard, often even harder than hardened tool steel, but are also very brittle especially at the edges. By accident knocking a coated part against a bench edge or other part can cause localized chipping of the coating to expose bare aluminium beneath. Such parts must be handled carefully and kept in trays or on racks with edges kept clear of other parts. They must not be bagged up loosely together for example. Fixtures etc. for subsequent machining or assembly must be designed such that they do not clamp into anodized surfaces wherever possible.
All of these factors can affect the quality of the adhered oxide layer. The anodic oxide layer is a robust solid but brittle material, and if it is subjected to sharp edges or snags then it can chip. However, if properly handled then anodized parts will look after themselves.